欢迎登录材料期刊网

材料期刊网

高级检索

  • 论文(89)
  • 图书()
  • 专利()
  • 新闻()

CRYSTAL DEFECTS AND GRAIN INTERFACE STRUCTURE OF ION-NITRIDED LAYERS

SUN Dongsheng LI Fengzhao Shandong Polytechnic University , Jinan , Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Academia Sinica , Shenyang , ChinaDAI Jiyan LI Douxing Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Academia Sinica , Shenyang , China associate professor , Institute of Materials Engineering , Shandong Polytechnic University , Jinan 250014 , China

金属学报(英文版)

Observation under high resolution electron microscope shows that the continuous bombing of high speed ions produces a great amount of vacant site defects.The assembly of vacancies forms vacant dish,and the collapase of vacant dish forms stacking fault tetrahedrons and oth- er crystal defects.The interfaces between phase ε(Fe_(2-3)N)and phase γ'(Fe_4N)are smooth, straight and coherent,and they have the orientation relationships of(11)//(0001)and [110]/[110] .

关键词: crystal defect , null , null , null

STRUCTURE AND SURFACE CONDITION OF ULTRAFINE AI PARTICLES

SUN Xiukui CHEN Wenxiu XU Jian FAN Xueshu WEI Wenduo State Key Laboratory of Rapidly Solidified Non-Equilibrium Alloys , Institute of Metal Research , Academia Sinica , Shenyang , ChinaWU Yukun PENG Yingguo Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Academia Sinica , Shenyang , China Associate Professor , Institute of Metal Research , Academia Sinica , Shenyang 110015 , China

金属学报(英文版)

The crystal habit,crystalline structure,surface condition and composition of the ultrafine Al particles prepared by inert gas evaporation method were studied in detail by means of high resolution transmission electron microscope,X-ray diffraction and X-ray photo-electron spectrum.The results indicate that the ultrafine Al particles prepared in high pure inert gas are of clear crystal habits,single crystal in a large majority and fcc crystalline structure with a_0=0.405 nm.It is also found on the surface of the Al particles that there is a layer of amor- phous Al_2O_3 with 2 nm average thickness,which could protect the particles against oxidizing further.Therefore,the ultrafine Al particles prepared by the inert gas evaporation method are very stable in atmosphere.

关键词: ultrafine Al particle , null , null , null

EFFECT OF SLIP ORIENTATION ON STRESS RESPONSE,INTERNAL FRICTION AND ULTRASONIC ATTENUATION DURING CYCLIC DEFORMATION IN Al SINGLE CRYSTALS

XIA Yuebo ZHANG Tianyi State Key Laboratory for Fatigue and Fracture of Materials , Institute of Metal Research , Academia Sinica , Shenyang , ChinaFEI Guangtao ZHOU Xing Laboratory of Internal Friction and Defects in Solids , Institute of Solid State Physics , Academia Sinica , Hefei , China Associate Professor , Institute of Metal Research , Academia Sinica , Shenyang 110015 , China

金属学报(英文版)

The variation of cyclic stress,internal friction and ultrasonic attenuation during cyclic deformation and relations among them have been investigated with different slip orientation Al single crystals.The results indicate that the value of cyclic stress σ,internal friction Q~(-1)and ultrasonic attenuation △α depend obviously on the slip orientation.There are large differences in above three parameters for different slip orientation Al crystals.In early stage of fatigue life,σ and △α increase and Q~(-1)decreases with cycles N,and △α reached maxi- mum before σ,while Q~(-1)and σ get the valley and the peak,respectively,at same cycles.

关键词: crystal orientation , null , null , null , null , null

END GRAIN ATTACK OF LD10CS PLATES DURING CHEMICAL MILLING

ZENG Xianghua , SHA Jiande , SU Ge Institute of Metal Research , Academia Sinica , Shenyang , ChinaYUAN Jigang LIU Fumei ZHONG Huiwen Southwest Aluminium Mill , China National Nonferrous Metals Industry Corporation , Chongqing , China SHA Jiande , Engineer , Institute of Metal Research , Academia Sinica , Shenyang , China

金属学报(英文版)

The end grain attack of LDIOCS aluminium alloy plates during chemical milling in hot aqueous solution of sodium hydroxide has been studied.The results show that the microsegregation of some components,i.e.Cu,Si etc.,is the main reason of the end grain at- tack,and it is affected by the conditions of heat treatment as well.The end grain attack significantly diminishes while some technical measures which are beneficial to the reduce of segregation were taken during melting and casting.

关键词: aluminium alloy , null , null , null

STRUCTURE OF Al-Mn-Zn-Mg ALLOY POWDER

WU Lijun , ZHAO Lihua , YANG Qiaoqin , LI Shaolu , LI Xieqian(Materials Research and Test Centre , Hunan University , Changsha 410082 , China)(Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Chinese Academy of Sciences , Shenyang 110015 , China)

金属学报(英文版)

The structure of Al-Mn-Zn-Mg alloy powder annealed at 800℃ has been studied by transmisston electron microscopy(TEM).An approximant phase(named as C-phase) to the decagonal phase was found and its crystal structure was determined It belongs to c-center orthorhombic lattice with a=2.35 nm,b=3.27 nm and c=1.22 nm.We stillfound a hexagonal phase with a=0.7) nm and c=0.79 nm,(named as phase) in the annealed alloy powder.The annealed alloy powder is composed of the C-phase,the phase,the decagonal phase and Al solid solution.

关键词: :quasicrystal , null , null

HYDROGEN PERMEATION AND DIFFUSION IN ALLOY INCOLOY 903

XU Jian SUN Xiukui CHEN Wenxiu LI Yiyi State Key Laboratory of RSA , Institute of Metal Research , Academia Sinica , China research assistant , Institute of Metal Research , Academia Sinica , Shenyang 110015 , China

金属学报(英文版)

Permeability and diffusivity of hydrogen in Fe-Ni-Co based superalloy lncoloy 903 were measured over the temperature range of 220 to 420℃ using a gaseous permeation technique. The effect of strengthening phase γ' precipitated after being aged on the hydrogen permeation and diffusion was investigated.It was indicated that the permeability and diffusivity of hydrogen in the alloy hardly depend on heat treatment condition and are not af- fected by γ' phase precipitated after being aged.The relationships between the permeability and diffusivity of hydrogen and the temperature can be respectively expressed as Φ=9.36×10~(-5)exp[-54.20(kJ/mol)/RT]mol/m·s·MPa~(1/2)and D=4.24×10~(-7)exp[-49.07(kJ/mol)/RT]m~2/s.

关键词: hydrogen permeation , null , null , null , null

FINE STRUCTURES OF BOTH INTERFACES AND INTERFACIAL REACTION PRODUCTS

LI Douxing PING Dehai NING Xiaoguang YE Hengqiang Laboratory of Atomic Imaging of Solids , Institute of Metal Research , Academia Sinica , Shenyang.China Professor , Institute of Metal Research , Academia Sinica , Shenyang 110015 , China

金属学报(英文版)

The characteristic of interface depending on the atomic structure exerts an inportant,and sometime controlling,influence on performance of the interacial materials. The present paper reviews the main studies on fine structure of both the materials inter- faces and interfacial reaction products in semiconductor uperlattice,metal multilayer ceram- ics and composite materials by mean of selected area electron doffraction patterns and high resolution electron microscopy. The following features of interfaces are reviewed:the orientation relationships;the char- acteristic of steps,facets and ronghness of interfaces;atomic bonding across the interface;the degree of coherency,the structure of misfit dislocations and elastic relaxations at the inter- faces:the presence of defects at the onterfaces:the structure of the interfacial reaction prod- ucts as well as the reaction kinetics and reaetion mechanism.

关键词: fine structure of the interfaces , null , null , null

IMPROVEMENT IN FATIGUE LIFETIME OF Ti-6Al-4V ALLOY BY CARBON IMPLANTATION

ZHANG Dawei YU Weicheng WANG Zhongguang National Laboratory for Fatigue and Fracture of Materials , Institute of Metal Research , Academia Sinica , Shenyang , China Associate Professor , Institute of Metal Research , Academia Sinica , Shenyang , 110015

金属学报(英文版)

Carbon ions with a dose of 3×10~(17) ions/cm~2 was implanted into Ti-6Al-4V alloy at an energy of 80 keV.A 28% increase in edurance limit was found with implantation under stress-controlled fatigue tests(R=O).The surface microstructure changes induced by ion implantation were identified using transmission electron microscopy(TEM).The feature of the fracture surface were observed on scanning electron microscope(SEM).The distribution profile of the implanted ions was measured by secondary ion mass spectroscopy(SIMS).The implanted surface layers contain a high density of irradiation defects and fine TiC precipitates.Subsurface crack origins were found in specimens either with or without implantation.The implanted species diffuse into matrix metal under the action of cyclic load- ing.A possible reason and mechanism for improving fatigue lifetime are also discussed.

关键词: surface modification , null , null

SOLUTION BEHAVIOUR OF VARIOUS ALLOYING ELEMENTS IN Ni_3Si

LI Yundong , ZHANG Tianxiang , ZHENG Zhi , ZHU Yaoxiao Institute of Metal Research , Academia Sinica , Shenyang , China Professor , Institute of Metal Research , Academia Sinica , Shenyang , China

金属学报(英文版)

The solid solubilities of 15 common alloying elements added to the Ll_2-type intermetallic compound Ni_3Si at 900°C have been estimated,and their substitution modes have been de- duced from the direction of solubility lobe of the compound.It is shown that the alloying behaviours in Ni_3Si are determined by both size and electronic factors,i.e.,the substitution mode is governed by electronic configuration and solubility by the both.An interaction parameter is presented to describe quantitatively the influence of electronic configuration on substitution mode and the solubility limit can be successfully explained together with atom radius.

关键词: alloying behaviour , null , null , null

  • 首页
  • 上一页
  • 1
  • 2
  • 3
  • 4
  • 5
  • 下一页
  • 末页
  • 共9页
  • 跳转 Go

出版年份

刊物分类

相关作者

相关热词